1.Thermal shock resistance,
2. High strength,
3. Good wear resistance,
4. Long service life.
Steel Fiber Castable Introduction
Steel Fiber Castable is produced by adding refractory steel fiber into the raw material to grant it a higher strength and thermal shock resistance, thus to finally increase its wear resistance capacity and service life. This castable is mainly used in the high-temperature wearable parts such as kilneye, feed opening, the wearable pier and the lining of power plant boiler.
Application of Steel Fiber Castable
. Steel furnaces
. Iron making furnaces
. Glass kiln
. Ceramic tunnel kiln
. Cement kiln
Steel Fiber Castable Technique Data
| Items | RS-F16 | RS-F16K | RS-F17 | |
| Al2O3+SiC% | 110℃x24h | 70 | 75 | 8 |
| Bulk Density g/cm 3 | 110℃x24h | 2.6 | 2.7 | 2.8 |
| MOR MPa | 1110℃x3h | 11 | 12 | 13 |
| 110℃x24h | 11 | 12 | 13 | |
| Cold Crushing Strength MPa | 1110℃x3h | 90 | 100 | 110 |
| 1110℃x3h | 90 | 100 | 110 | |
| Linear Dimensional Change % | 110℃x24h | ±0.1 | ±0.1 | ±0.1 |
| 1110℃x3h | ±0.3 | ±0.3 | ±0.3 | |